Best properties for lowest cycle times
Thermodur 2383 Supercool is the tool steel that combines excellent mechanical properties and high wear resistance with very high thermal conductivity. This makes this special steel ideally suitable for application in indirect press hardening, die casting, and injection molding tools.
Thermodur 2383 Supercool, quenched and tempered to 45 HRC, features a significantly higher thermal conductivity compared to conventional hot work tool steels like 1.2343 (H11), 1.2344 (H13), and 1.2367 at similar hardness level. A maximum value of 44 W/ (m K) is reached at 100 °C. A mold insert made of this special steel thus can dissipate heat in a controlled manner within a very short time.
The result: a tool made of Thermodur 2383 Supercool noticeably lowers the cycle times in molding/forming applications thanks to improved heat conductivity.
Contact
Michaela König
Telefon: +49 (0) 2302 29-4391
Send E-Mail